Publications of T. Schwarz-Selinger
All genres
Journal Article (203)
81.
Journal Article
522, pp. 158 - 167 (2019)
Isolating the detrapping of deuterium in heavy ion damaged tungsten via partial thermal desorption. Journal of Nuclear Materials 82.
Journal Article
440, pp. 202 - 205 (2019)
Corrigendum to "Optimization of the depth resolution for deuterium depth profiling up to large depths" [Nucl. Instrum. Methods Phys. Res. B 387 (2016) 103–114]. Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms 83.
Journal Article
507, pp. 54 - 58 (2018)
Deuterium absorption in reduced activation ferritic/martensitic steel F82H under exposure to D2O vapor/water at room temperature. Journal of Nuclear Materials 84.
Journal Article
89, 103501 (2018)
SIESTA: A high current ion source for erosion and retention studies. Review of Scientific Instruments 85.
Journal Article
511, pp. 560 - 566 (2018)
Deuterium permeation behavior and its iron-ion irradiation effect in yttrium oxide coating deposited by magnetron sputtering. Journal of Nuclear Materials 86.
Journal Article
58, 066005 (2018)
Motion of W and He atoms during formation of W fuzz. Nuclear Fusion 87.
Journal Article
58, 056027 (2018)
Influence of sub-surface damage evolution on low-energy-plasma-driven deuterium permeation through tungsten. Nuclear Fusion 88.
Journal Article
17, pp. 228 - 234 (2018)
Influence of the presence of deuterium on displacement damage in tungsten. Nuclear Materials and Energy 89.
Journal Article
430, pp. 42 - 46 (2018)
Fluence dependent changes of surface morphology and sputtering yield of iron: Comparison of experiments with SDTrimSP-2D. Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms 90.
Journal Article
508, pp. 139 - 146 (2018)
Sputtering of polished EUROFER97 steel: Surface structure modification and enrichment with tungsten and tantalum. Journal of Nuclear Materials 91.
Journal Article
512, pp. 25 - 30 (2018)
The influence of helium on deuterium retention in beryllium co-deposits. Journal of Nuclear Materials 92.
Journal Article
12, pp. 678 - 682 (2017)
D retention in Be exposed to fusion relevant mixed species D2-He plasma. Nuclear Materials and Energy 93.
Journal Article
57, 086015 (2017)
Influence of near-surface blisters on deuterium transport in tungsten. Nuclear Fusion 94.
Journal Article
12, pp. 468 - 471 (2017)
Erosion of Fe-W model system under normal and oblige D ion irradiation. Nuclear Materials and Energy 95.
Journal Article
57, 116041 (2017)
Plasma-wall interaction studies within the EUROfusion consortium: progress on plasma-facing components development and qualification. Nuclear Fusion 96.
Journal Article
495, pp. 211 - 219 (2017)
Surface modifications and deuterium retention in polycrystalline and single crystal tungsten as a function of particle flux and temperature. Journal of Nuclear Materials 97.
Journal Article
57, 046028 (2017)
Mitigated blistering and deuterium retention in tungsten exposed to high-flux deuterium-neon mixed plasmas. Nuclear Fusion 98.
Journal Article
T170, 014010 (2017)
Preparation of erosion and deposition investigations on plasma facing components in Wendelstein 7-X. Physica Scripta 99.
Journal Article
12, pp. 372 - 378 (2017)
Quantitatively measuring the influence of helium in plasma-exposed tungsten. Nuclear Materials and Energy 100.
Journal Article
T170, 014057 (2017)
The effect of high energy ion beam analysis on D trapping in W. Physica Scripta